Ricoh DD5450 plate paper wrinkling in the printing process

Visitor 284 0
SymptomsDD5450 plate making is normal. When printing reaches about 30 sheets, the paper begins to wrinkle.                                Cause analysis1. It is preliminarily judged that the installation of the steel mesh is loose or the steel mesh has cracks, but this factor is ruled out after inspecting the steel mesh.

2. Observe that the wrinkling position of the paper is in the center of the paper, and the direction of the wrinkling is almost parallel to the feeding direction, which matches the position of the feeding roller.

3. After adjusting (reducing) the feed separation pressure, the fault was eliminated. Therefore, it is determined that during the paper feeding process, the high separation pressure causes the tension at the center of the paper to be greater than at both ends. This type of paper has an impact on the printing process (wrinkling).



SolutionAdjusting the separation pressure to the appropriate position can solve the problem.
NoteRemind customers not to adjust the separation pressure arbitrarily.